Chloride profiles measured on concrete cores collected from the 15 blocks placed at the Fehmarnbelt exposure site are presented below. The profiles were measured after about two years (735 days) of exposure to the marine environment, and for each type of concrete, two cores were drilled, i.e. one from below sea level and one from the splash zone.

All profiles were measured according to the method described in DS 423.28:1984  Testing of concrete – Hardened concrete – Chloride content, and the data presented below have not been corrected for variations in aggregate packing near the concrete surface.

Fehmarn concrete A_chloride profiles_ 2 years

Fehmarn concrete B_chloride profiles_ 2 years

Fehmarn concrete C_chloride profiles_ 2 years

Fehmarn concrete D_chloride profiles_ 2 years

Fehmarn concrete E_chloride profiles_ 2 years

Fehmarn concrete F_chloride profiles_ 2 years

Fehmarn concrete G_chloride profiles_ 2 years

Fehmarn concrete H_chloride profiles_ 2 years

Fehmarn concrete I_chloride profiles_ 2 years

Fehmarn concrete J_chloride profiles_ 2 years

Fehmarn concrete K_chloride profiles_ 2 years

Fehmarn concrete L_chloride profiles_ 2 years

Fehmarn concrete M_chloride profiles_ 2 years

Fehmarn concrete N_chloride profiles_ 2 years

Fehmarn concrete O_chloride profiles_ 2 years